Refurbishing concrete
- DEMOLITION
Removal of flaking concrete and thorough cleaning (until the iron is bared) of the reinforcing iron.
- TREATMENT FOR THE IRON
Reinforcing iron treated with rust-inhibiting mortar such as AKRON-FER by Technokolla, to be applied with a brush.
Amount required:
120-150 g/ml AKRON-FER
- REFURBISHING CONCRETE
Refurbishing of the layer covering the reinforcing rods using fiber-reinforced mortar with compensated shrinkage such as AKRON or AKRON-R (rapid), in coats up to 3 cm thick or, alternatively, AKRON-FLUID or GAP in coats up to 5 cm thick.
Amount required:
18-19 Kg/m2 AKRON, AKRON-R or AKRON-FLUID for every cm of thickness
16-18 kg/m2 GAP for every cm of thickness
- FINISH
Finishing layer for the refurbished concrete using non-carbonating skimming plaster specially formulated for protecting concrete, such as AKRON-F by Technokolla, in coats up to 3 mm thick.
Amount required:
1.65 kg/m2 AKRON-F for every mm of thickness
|
 |

|